Beryllium Copper Alloy
-
C17200 Beryllium Copper
-
C17300 Beryllium Copper
-
C17510 Beryllium Copper
-
C17500 Beryllium Copper
-
Chromium Zirconium Copper
-
Dispersion Strengthened Copper
-
Beryllium Copper Wire
-
Beryllium Copper Sheet
-
Beryllium Copper Rods
-
Beryllium Copper Strip
-
Beryllium Copper Tube
-
Tellurium Copper Alloy
C18150 CuCr1Zr Chromium Zirconium Copper Bars With High Electrical And Thermal Conductivity
Contact me for free samples and coupons.
Whatsapp:0086 18588475571
Wechat: 0086 18588475571
Skype: sales10@aixton.com
If you have any concern, we provide 24-hour online help.
xName | Chromium Zirconium Copper Bars | Grade | C18150 CuCr1Zr |
---|---|---|---|
Specification | As The Requirement Of Customers' | Advantage | With High Electrical And Thermal Conductivity |
Safe Handling | No Special Health Risk | Machining Property | Good |
Density G/cm³ | 8.89 | Cu(Min) | Standard |
Export To | All Over The World | ||
High Light | c18150 copper chromium zirconium,c18150 chromium zirconium copper |
C18150 CuCr1Zr Chromium Zirconium Copper Bars With High Electrical And Thermal Conductivity
Product Normal Description:
Product Name | Chromium Zirconium Copper Bars |
---|---|
Grade: | C18150 CuCr1Zr |
Standard: | RWMA Class 2, DIN 2.1293, CW106C to EN |
Product Specification: | we could provide beryllium copper alloy according customers' requirement. |
Delivery Time: | Usually within 10~15 days |
Package: |
Packed in woodencases |
Product Brand: | CUBERYLLIUM® |
CuCr1Zr – UNS.C18150 Chromium Zirconium Copper C18150 is an excellent and unique copper alloy with high electrical conductivity, hardness, and ductility, moderate strength, and excellent resistance to softening at elevated temperatures. The addition of 0.1% zirconium (Zr) and 1.0% chromium (Cr) to copper results in a heat treatable alloy which may be solution treated and subsequently aged to produce these desirable properties. Rod is usually supplied from the mill in the fully aged and drawn condition so no further heat treatment is required by the fabricator. The softening temperature of properly heat treated C18150 rod exceeds 500°C as compared to unalloyed pure copper which softens at 200°C, and silver bearing coppers which soften at 350°C.
Furthermore, many evidences shows that C18150 can provide less sticking and resisting deformation longer than its C18200 counterpart in some specific situatons.
Chemical Composition of C18150 CuCr1Zr Chromium Zirconium Copper Alloys:
Product Grade: CUBERYLLIUM ®-815 (UNS.C18150)
Cr | 0.50-1.50% |
Zr: | 0.05-0.25% |
Cu: | Balance |
Note: Copper plus additions equal 99.7% minimum. |
Typical Physical Properties of C18150 CuCr1Zr Chromium Zirconium Copper Alloys:
Metric Units | Imperial Units | |
---|---|---|
Density | 8.89 gm/cm³ @ 20°C | 0.321 lb/in³ @ 68°F |
Specific Gravity | 8.89 | 8.89 |
Melting Point (Liquidus) | 1080°C | 1976°F |
Melting Point (Solidus) | 1070°C | 1958°F |
Coefficient of Thermal Expansion | 16.45 x 10 -6 / °C (20-300°C) | 9.5 x 10 -6 / °F (68-392°F) |
Themal Conductivity | 323.9 W/m. °K @ 20°C | 187.0 BTU/ft²/ft/hr/°F @ 68°F |
Electrical Conductivity | 0.464 MegaSiemens/cm @ 20°C | 80% IACS@ 68°F |
Modulus of Elasticity (tension) | 117,200 MPa | 17,000ksi |
Note:
1: the units are based upon US Customary.
2: the typical physical properties apply to age hardened products.
Typical Uses For C18150 CuCr1Zr Chromium Zirconium Copper Alloys: | |
Industrial: | Welding Wheels, Tips and Rod extensions for resistance seam and spot welding |
Electrical Industry: | Resistance Welding Electrodes, Circuit Breaker Switches. |
Consumer: | Rod Extensions, Pencil-type, Light Soldering Guns, Tip |
Product Photos: